The process of fusing and slumping glass begins with deciding on the mold for the specific project. The glass colors are then chosen and cut to fit the mold. Once the design is created and all the pieces are carefully placed they are fused in the kiln for approximately 30 hours. The fused glass is then put on the chosen mold and put back into the kiln to slump for another 30 plus hours. The finished pieces can be used or attractively displayed in the home.